- EN26 EN26W Alloy Steel round bar
- EN26 EN26W Alloy Steel forging
- EN26 EN26W Alloy Steel sheet
- EN26 EN26W Alloy Steel flat bar
- EN26 EN26W Alloy Steel pipe
EN26 EN26W Alloy Steel
Production specification
Square-shape steel: 1mm to 4000mm
Plate steel:0.1mm to 4000mm
Width: 10mm to 2500mm
Lenth: We can supply any lenth based on the customer's requirement.
Forging: Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes
Tubings: OD: φ6-1800mm, with wall thickness ranging from 1-35 mm.
Finished goods condition: hot forging/hot rolling + annealing/normalizing + tempering/quenching + tempering/any conditions based on the customer's requirement
Surface conditions: scaled (hot working finish)/ground/rough machining/fine machining/based on the customer's requirement
Furnaces for metallurgical processing: electrode arc + LF/VD/VOD/ESR/Vacuum consumable electrode.
Ultrasonic inspection: 100% ultrasonic inspection for any inperfections or based on the customer's requirementExcellent service for all kinds of industries,with advantages of technologies, equipment and price.
We serve you with our honesty, integrity, and professionality.
EN26 EN26W Alloy Steel
EN26 is a 2.5% nickel chromium molybdenum high tensile steel, usually supplied hardened and tempered to either 'V' or 'W' condition. EN26 is suitable for applications which require higher tensile and yield strength than EN24 or EN25 specifications. EN26 round bar is available from stock. When required EN26 can be induction or flame hardened. EN26 can also be nitrided. |
TYPICAL ANALYSIS |
EN26 |
|
|||
C. |
Si. |
Ni. |
Cr. |
Mo. |
|
0.40% |
0.30% |
0.60% |
2.50% |
0.75% |
0.55% |
Mechanical Properties EN26
Heat |
Tensile |
Yield |
a% on |
Impact |
Impact |
Proof |
Hardness |
Size |
V |
1000/1150 |
835 |
12 |
34 |
28 |
820 |
293/352 |
>29≤250
|
V |
1000/1150 |
850 |
12 |
47 |
42 |
835 |
293/352 |
>29≤150 |
W |
1075/1225 |
925 |
11 |
27 |
22 |
910 |
311/375 |
>29≤250 |
W |
1075/1125 |
940 |
11 |
40 |
35 |
910 |
311/375 |
>29≤250 |
Forging
Heat to 1150 to 1200°C and hold at temperature until throughly soaked and suitable to forge. Do not forge below 850°C.
Heat Treatment
To harden EN26 first heat the component to 820 to 850°C and hold at temperature until throughly soaked. Quench the EN26 component in oil, water or polymer as required. EN26 can be flame or induction hardened to achieve a high surface hardness.
Tempering
To temper EN26 heat the component to the required tempering temperature (450 to 660°C), thoroughly soak for 1 hour per 25mm thickness of section, cool in air.
Nitriding
EN26 can be nitrided to give a surface hardness of up to 60HRc. Heat to 500 to 530°C and hold for sufficient time to develop the case depth required, no quenching is required.
Stress Relieving
To stress relieve EN26 heat the component to 640 to 660°C and hold until temperature is uniform through the section. Soak the EN26 component for 1 hour per 25mm thickness of section and cool in air.
Mechanical properties