- 1.7006, DIN 46Cr2, AISI 5045 round bar
- 1.7006, DIN 46Cr2, AISI 5045 forging
- 1.7006, DIN 46Cr2, AISI 5045 sheet
- 1.7006, DIN 46Cr2, AISI 5045 flat bar
- 1.7006, DIN 46Cr2, AISI 5045 pipe
1.7006, DIN 46Cr2, AISI 5045
Production specification
Square-shape steel: 1mm to 4000mm
Plate steel:0.1mm to 4000mm
Width: 10mm to 2500mm
Lenth: We can supply any lenth based on the customer's requirement.
Forging: Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes
Tubings: OD: φ6-1800mm, with wall thickness ranging from 1-35 mm.
Finished goods condition: hot forging/hot rolling + annealing/normalizing + tempering/quenching + tempering/any conditions based on the customer's requirement
Surface conditions: scaled (hot working finish)/ground/rough machining/fine machining/based on the customer's requirement
Furnaces for metallurgical processing: electrode arc + LF/VD/VOD/ESR/Vacuum consumable electrode.
Ultrasonic inspection: 100% ultrasonic inspection for any inperfections or based on the customer's requirementExcellent service for all kinds of industries,with advantages of technologies, equipment and price.
We serve you with our honesty, integrity, and professionality.
1.7006, DIN 46Cr2, AISI 5045
Designation by Standards
Brand Name | LH No. | Mat. No. | DIN | EN | AISI |
46CR2 | 788 | 1.7006 | 46Cr2 | - | 5045 |
Chemical Composition (in weight %)
C | Si | Mn | Cr | Mo | Ni | V | W | Others |
0.46 | <0.40 | 0.65 | 0.50 | - | - | - | - | - |
Description
Special structural steel.
Applications
Low and moderately stressed components for automobile industry and mechanical engineering - shafts, connecting rods, crankshafts.
Physical properties (avarage values) at ambient temperature
Modulus of elasticity [103 x N/mm2]: 210
Density [g/cm3]: 7.85
Soft Annealing
Heat to 650-700oC, cool slowly. This will produce a maximum Brinell hardness of 223.
Normalizing
Temperature: 840-880oC.
Hardening
Harden from a temperature of 820-860oC followed by oil or water quenching.
Tempering
Tempering temperature: 540-680oC.
Mechanical Properties in Quenched and Tempered Condition
Diameter (mm) | 0.2 proof stress (N/mm2) | Tensile stregth (N/mm2) | Elongation (%) | Reduction (%) | Impact energy (J) |
Up to 16 | 650 | 900-1100 | 12 | 35 | 30 |
17-40 | 550 | 800-950 | 14 | 40 | 35 |
41-100 | 400 | 650-800 | 15 | 45 | 35 |
Diagram Tempering Temperature - Mechanical Properties
Forging
Hot forming temperature: 1100-850oC.
Machinability
No data.
Mechanical properties
Heat treatment
Machining
Welding performance
Related hot word search:1.7006 DIN 46Cr2 AISI 5045 round bar 1.7006, DIN 46Cr2, AISI 5045,forging 1.7006, DIN 46Cr2, AISI 5045,1.7006, DIN 46Cr2, AISI 5045 sheet,coil 1.7006, DIN 46Cr2, AISI 5045,1.7006, DIN 46Cr2, AISI 5045 flat bar,pipe 1.7006, DIN 46Cr2, AISI 5045,1.7006, DIN 46Cr2, AISI 5045 Lrregular
Prev:1.7227, DIN 42CrMoS4, AISI 4140
Next:1.6773, DIN 36NiCrMo16