- 1.5122, DIN 37MnSi5 round bar
- 1.5122, DIN 37MnSi5 forging
- 1.5122, DIN 37MnSi5 sheet
- 1.5122, DIN 37MnSi5 flat bar
- 1.5122, DIN 37MnSi5 pipe
1.5122, DIN 37MnSi5
Production specification
Square-shape steel: 1mm to 4000mm
Plate steel:0.1mm to 4000mm
Width: 10mm to 2500mm
Lenth: We can supply any lenth based on the customer's requirement.
Forging: Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes
Tubings: OD: φ6-1800mm, with wall thickness ranging from 1-35 mm.
Finished goods condition: hot forging/hot rolling + annealing/normalizing + tempering/quenching + tempering/any conditions based on the customer's requirement
Surface conditions: scaled (hot working finish)/ground/rough machining/fine machining/based on the customer's requirement
Furnaces for metallurgical processing: electrode arc + LF/VD/VOD/ESR/Vacuum consumable electrode.
Ultrasonic inspection: 100% ultrasonic inspection for any inperfections or based on the customer's requirementExcellent service for all kinds of industries,with advantages of technologies, equipment and price.
We serve you with our honesty, integrity, and professionality.
1.5122, DIN 37MnSi5
Designation by Standards
Brand Name | LH No. | Mat. No. | DIN | EN | AISI |
VMS135 | 707 | 1.5122 | 37MnSi5 | - | - |
Chemical Composition (in weight %)
C | Si | Mn | Cr | Mo | Ni | V | W | Others |
0.37 | 1.25 | 1.25 | - | - | - | - | - | - |
Description
Structural steel. Parts of high core stability and good toughness like gear parts etc.
Applications
Low and moderately stressed components for vehicles, machines and engines.
Physical properties (avarage values) at ambient temperature
Modulus of elasticity [103 x N/mm2]: 210
Density [g/cm3]: 7.85
Thermal conductivity [W/m.K]: 25.0
Coefficient of Linear Thermal Expansion 10-6 oC-1
20-100oC | 20-300oC | 20-500oC |
11.1 | 12.9 | 13.9 |
Continuous Cooling Transformation (CCT) Diagram
Soft Annealing
Heat to 680-720oC, cool slowly. This will produce a maximum Brinell hardness of 217.
Normalizing
Temperature: 860-890oC.
Stress Relieving
Stress relieving to remove machining stresses should be carried out by heating to 120-200oC, holding for one hour at heat, followed by air cooling. This operation is performed to reduce distortion during heat treatment.
Hardening
Harden from a temperature of 820-850oC followed by water or oil quenching. Hardneess after quenching is 52-54 HRC.
Tempering
Tempering temperature: 480-60oC, air.
Forging
Hot forming temperature: 1050-850oC.
Machinability
Machining is best done with this alloy in the annealed or normalized and tempered condition. It can be machined by all conventional methods.
Corrosion Resistance
This is a low steel/" target="_blank" class="keylink">alloy steel and not a corrosion resistant alloy. Protective coating should be used.
Welding
The alloy can be fusion or resistance welded. Preheat and post heat weld procedures should be followed when welding this alloy by established methods.
Cold working
The VMS135 alloy may be cold worked, in the annealed condition, by conventional methods and tooling. It has good ductility.
Mechanical properties
Heat treatment
Machining
Welding performance
Related hot word search:1.5122 DIN 37MnSi5 round bar 1.5122, DIN 37MnSi5,forging 1.5122, DIN 37MnSi5,1.5122, DIN 37MnSi5 sheet,coil 1.5122, DIN 37MnSi5,1.5122, DIN 37MnSi5 flat bar,pipe 1.5122, DIN 37MnSi5,1.5122, DIN 37MnSi5 Lrregular
Prev:1.7182, DIN 27MnCrB5-2
Next:1.5223, DIN 42MnV7